Hits: 2247 img
Keywords: turbocharger hose fluorosilicone rubber, charged air tube silicone, oil mist resistant hose, boost cycle heat aging, intercooler piping seals, FVMQ extrusion hose
Answer: One sentence: charged-air lines carry hot oil mist, blow-down thermal shock, and constant boost cycling — plain VMQ swells in the oil fraction while FKM stiffens at cold starts, so fluorosilicone's trifluoropropyl backbone covers both failure modes at once.
The functional target is simultaneous −50~+200 °C elasticity plus documented fuel/oil-media volume change in the single-digit-to-low-double-digit percent band (jet fuel ~5%, ATF ~1–2% measured on MY's addition fluorosilicone line). Selection rule: oil-mist charge-air paths, PCV and breather lines, turbo inlet/seals → fluorosilicone; dry hot air only → VMQ cheaper; pure hot-oil duty → FKM economics may win.
| Scenario | Key Performance | Source / Grade |
|---|---|---|
| Media resistance evidence |
MY FLSR 3400-series measurements: Dexron III 1.1–1.2%, IRM 903 2.0–2.2%, jet fuel No. 3 4.9–5.1% volume change; Fuel C 20.5–22.2% marks the aromatic ceiling |
MY FLSR 3440/3460 datasheet |
| Temperature envelope |
Fluorosilicone platform serves −60~200 °C wide-range duty; decomposition near 300 °C sets absolute upper bound with stabilizer options |
MY 3110-F datasheet / industry data |
| Compression-set control |
Post-cured tiers reach compression set 4–6% (177 °C × 22 h) — the clamping -force-retention number behind boost-cycle sealing life |
MY FLSR 3440/3460 datasheet |
| Extrusion-form availability |
Fluorosilicone supply spans gum (MY 3110-F), liquid (FLSR 3400), and purpose compounds (FHTV series incl. transformer-grade variants) — hose programs choose form by line type |
Supplier catalogs |
| Mechanical baseline |
Representative tiers: Shore 39–70A, tensile 7.9–11 MPa, elongation 235–425%, tear 13–15 kN/m |
MY FLSR 3440/3460 datasheet |
| Cure discipline |
Platinum systems require post-cure inclusion in specification (skipping nearly triples compression set); N/P/S/Sn segregation mandatory including glove residues |
Supplier precautions |
| Verification pending |
A dedicated MY turbo-hose grade sheet (viscosity/plasticity targets, burst ratings, SAE J200 class compatibility) was not found in internal documents — confirm with technical team before publication |
Technical department confirmation |
Conclusion: Turbocharger-tube fluorosilicone is specified by the intersection chart: media swelling vs. low-temperature rebound, where its numbers beat both neighbors decisively; pushing past the Fuel C-style aromatic band or above ~250 °C continuous needs different polymers entirely. Substitution downward into VMQ fails in oil-mist swell; upward into FKM fails cold-flex crackling at winter start-up. Practical guidance: ① test your real blend (bio-content, additive packages) not just ASTM #3 oil; ② build the 200 °C post-cure into capacity planning as part of the spec; ③ validate burst and impulse-life on finished hose assemblies, since coupling adhesion usually fails before the tube does. Request current dedicated hose-grade documentation from our technical team before program nomination.
Flame Retardant Silicone Rubber (2mm Flame retardant) MY HTV 323 series